dieselpower
Active Member
Got a job to do next week, it's a re-roughcast on a new build.
The story is, it was a hpx base coat, then a dash receiver with a wet dash roughcast.
However, the feckwits that done it after beading and hpx then proceeded to render the rest of building with dash receiver. Leave it for a week and come back and roughcast onto set receiver..
It looked awful and obviously is not what the client asked for.
I have taken it back to hpx and I'm going to score it, k-rend rep said prime it with r7( which I have just realized is SBR) now did he mean with r7 alone or diluted with water, or mixed with something else??
The story is, it was a hpx base coat, then a dash receiver with a wet dash roughcast.
However, the feckwits that done it after beading and hpx then proceeded to render the rest of building with dash receiver. Leave it for a week and come back and roughcast onto set receiver..
It looked awful and obviously is not what the client asked for.
I have taken it back to hpx and I'm going to score it, k-rend rep said prime it with r7( which I have just realized is SBR) now did he mean with r7 alone or diluted with water, or mixed with something else??