  1. G

    Hp12

    Hi got a render job . After painstakingly taking off defective render . It’s left brickwork in varied state of repair . Most good but Some lime motar other extended areas in hard sand cement masonry . Mostly flat it only ever had a single coat of render with a painted stipple or Terylene finish...
  2. B

    K rend tc primer

    Need some advice We’re currently doing a k rend job (TC system) It’s 10m2 and 28 degree heat We’ve applied the primer 24 hours after finishing the hp12 hoping to just finish it tomorrow The client is a complete nightmare and has data sheet at hand saying 14days Can we wash off the primer...
  3. S

    Hp12 base

    Might be a stupid question. But can I put on my first pass of hp12, run through with serated edge. Then bed my mesh in. Next day, hp12 over it and , level, spat, sponge etc. Bringing it out to the beads. Ready for top coat. Having trouble doing big gable ends all in one hit, but worried if I...
  4. G

    k-rend hp12 single coat?

    Hi, I'm new on here and would like some advice please! Would k-rend hp12 suffice as a one and only finish coat? This would be on top of block work with mesh. Single coat of hp12, stippled, then 2 coats of paint. Would this be satisfactory? K-rend recommend their finishing coat of kmix GP...
Back
Top