Do you lads who do the last few trowels with the plastic do a cross trowel with steel once the wall have picked up a bit or just finish by plastic?
 
I been using it for a few weeks. So much easier. I flatten with the steel trowel then 3 trowels with the plazi. Bloody maaaarvelous
 
Speedskim straight after laying on, plastic trowel 5-10 later. s*p*r*lex with water 40 mins later,plastic trowel 5-10 later. s*p*r*lex once set has darkened to give slight polish.

Mpfinish one coat but works the same on bg board finish just a bit harder.
 
Speedskim straight after laying on, plastic trowel 5-10 later. s*p*r*lex with water 40 mins later,plastic trowel 5-10 later. s*p*r*lex once set has darkened to give slight polish.

Mpfinish one coat but works the same on bg board finish just a bit harder.
 