got a job, goin over moisture res. plasterboard.
wat wud u prep the board with? coat of pva?
thinkin about using board finish due to lack of suction?
cheers chaps
 
pva it or gypbond it ...............yeh i'd deffo use board finish multi will never last on that background no sir ;D
 
spunky said:
you can use wba but you need to mix multi and board finish 50/50

Plus use warm water when mixing 50/50 helps strengthen the molecular structure during the chemical reaction of the plaster.
 
i used to work with an old hand that did that ....dont see it happening nowadays shame everyones just interested in the money >:(
 
skim them ... we have done loads of it and havent had any come backs ever .... mind you I did change my phone number .....
 
kirk johnstone said:
Chris W said:
kirk johnstone said:
thistle gyp prime ;)
Link Removed

???

haha i only posted this because it would be funny when someone goes to buy it and they get the price :D :D :D £70+ ;D


Now the other day you were saying people should only post helpful comments, or are you just going to say "it was for a laugh" every time you get something wrong? ???
 
essexandy said:
kirk johnstone said:
Chris W said:
kirk johnstone said:
thistle gyp prime ;)
Link Removed

???

haha i only posted this because it would be funny when someone goes to buy it and they get the price :D :D :D £70+ ;D


Now the other day you were saying people should only post helpful comments, or are you just going to say "it was for a laugh" every time you get something wrong? ???

you know what andy your right mate so i have removed the posts. sorry lads. now dont i look like a tit :(
 
you are a tit. this is my point mate. people get their answers but you have to take the banter with it.
 
They didn't use gyp prime 100 years ago so it won't be in kirks book surprised he never told you to 3 x1 sand cement it though ha ha
 
ha thanks pwi, what really happened was i was ment to write thistle bond it but got mixed up and said gyp prime instead then when chriss w spotted it and pointed it out i thought i would try and make it look like i did it on purpose for a laugh and then that made it worse because i contradicted what i was saying the other day. :-\

i am going to log off and go an sit in the corner ::)
 
your a little monkey you are steve ;D

its been ok had about five phone calls for work so thats been good but had a good hangover all day, how about you have you done any more polished stuff?
 
nope, my nephews birthday and they live in huddersfield so been there all day. didnt get back till 9. ill prime it tomorrow and do the rest monday. pics up monday night. got 1 job for next week. a ceiling to overskim after some pikey f**k*d it up. s**t one.
 
ellesmere port, its in between liverpool and chester i think you are about 100 or so miles away..... coffee two sugar's and the missus drinks tea
 
liverpools over 2hours away from me mate so ring me when your near, don't want it to get cold!
 
f**k knows mate, anyway im off, just seen a van on ebay thats local so gonna get up early and have a look tomorrow. night sweetie xx ;D
 
spunky said:
pva it or gypbond it ...............yeh i'd deffo use board finish multi will never last on that background no sir ;D
spunky thought gypbond was for high suction mr boards are surely not much suction hence i dont think pva would be sutable either they recomend thistle bond it to form a key here we go lol
 
exactly dont get it why cut corners why not just use the right product for the right application were not payin for it the customer is
 