Hi guys and gals
Do mainly internal stuff but have a job at my own home that I fancy trying k rend on. Small front wall.approx 700 high and 1600mm wide so ideal to start on and it's my own gaff so theres no customers to please .

Have a few questions as not used the stuff before
Was gonna sbr then basecoast with hp12 then top off with krend and use scratcher to finish.

Wall is out 3/4 inch front top to bottom. Will the hp12 cope with dubbing out this far ? I suppose I could do it in stages

Also for a wall so small will I need a small h bar to flatten or will a hand scratcher be enough.

Does the top coat need two coats as I've seen on YouTube it needs a wet on wet two coat topcoat ??
Would a spat be fine to rule of the top coat or is that not necessary

Cheers
 
Hi guys and gals
Do mainly internal stuff but have a job at my own home that I fancy trying k rend on. Small front wall.approx 700 high and 1600mm wide so ideal to start on and it's my own gaff so theres no customers to please .

Have a few questions as not used the stuff before
Was gonna sbr then basecoast with hp12 then top off with krend and use scratcher to finish.

Wall is out 3/4 inch front top to bottom. Will the hp12 cope with dubbing out this far ? I suppose I could do it in stages

Also for a wall so small will I need a small h bar to flatten or will a hand scratcher be enough.

Does the top coat need two coats as I've seen on YouTube it needs a wet on wet two coat topcoat ??
Would a spat be fine to rule of the top coat or is that not necessary

Cheers
Levelothe wall shouldn’t be a problem, but not necessarily really.
 
To sell more mesh, thats why, unless its at stress points say above door/ window, waste of time and cash.
 
Hi guys and gals
Do mainly internal stuff but have a job at my own home that I fancy trying k rend on. Small front wall.approx 700 high and 1600mm wide so ideal to start on and it's my own gaff so theres no customers to please .

Have a few questions as not used the stuff before
Was gonna sbr then basecoast with hp12 then top off with krend and use scratcher to finish.

Wall is out 3/4 inch front top to bottom. Will the hp12 cope with dubbing out this far ? I suppose I could do it in stages

Also for a wall so small will I need a small h bar to flatten or will a hand scratcher be enough.

Does the top coat need two coats as I've seen on YouTube it needs a wet on wet two coat topcoat ??
Would a spat be fine to rule of the top coat or is that not necessary

Cheers
I have spare mesh if you live near Farnham Hampshire
 
So lads can you dub out 3/4 I ch with hp12 and do I need to spat top coat a d is it a 2 coat top coat
 
Love forums
Post a question
Odd sarky comment
Start argument
One nice guy offers free materials
No one answers the questions...

Cheers lads
would dub it out you want to see the s**t that’s gone down at my house. Or s/c scratch to bring it out?
 
Hi guys and gals
Do mainly internal stuff but have a job at my own home that I fancy trying k rend on. Small front wall.approx 700 high and 1600mm wide so ideal to start on and it's my own gaff so theres no customers to please .

Have a few questions as not used the stuff before
Was gonna sbr then basecoast with hp12 then top off with krend and use scratcher to finish.

Wall is out 3/4 inch front top to bottom. Will the hp12 cope with dubbing out this far ? I suppose I could do it in stages

Also for a wall so small will I need a small h bar to flatten or will a hand scratcher be enough.

Does the top coat need two coats as I've seen on YouTube it needs a wet on wet two coat topcoat ??
Would a spat be fine to rule of the top coat or is that not necessary

Cheers
Why use k rend
 
Back
Top