All float finish renders suffer from rapid dehydration when finishing in the sun or wind. Stopping the moisture escaping to quickly is as simple a fix as pulling a drop film down from the soffit onto the render as you go, or a couple of light mists of water whilst you're loading up.
 
This one time, mid summer we did a rather large building in sand and cement and to stop it drying out too fast we hung hessian from the scaff and soaked it. Works well.
 
One thing i learned about render product over 15 years ago.
Never never ever take technical advice from a merchant. Ever.
They are salesmen and nothing more

Cpi is a 2 coat render so is kmix. Wether it can be done or has been done successfully its a 2 coat system. Ocr is a one coat product its composition will be different. No matter buildbase swearing blind kmix is equal - its different

On the thickness 10mm is ok as long as the finishing coat it the acrylic texture finish such as dpr, weber sil, tc15 etc.

Yeah mate all mine like that woukd be getting acrylic on top of , its the way ive been shown ... Happy you said that :-) lol
 