Doesn’t always need the hard 1 at the end, just depends how the multi finish dries outFour trowels as standard? f**k that!
Doesn’t always need the hard 1 at the end, just depends how the multi finish dries outFour trowels as standard? f**k that!
100% agree I do the same there maybe times where it might need more than 2 trowels I dont need to flatten it as such as I lay it on nice and neat anyway scrape any s**t of the ceiling line and angles leave it to pick up abit trickle of water on the edges and angles then 1st trowel leave it to pick up abit more water on the edges and angles again 2nd trowel and it's done really polishing the wall is optional really some times I do sometimes I dontYes sometimes just the two. No speedskim, just put on and laid in neatly and two passes with an MT Permashape.
It gets exactly how many it needs to achieve the right finish, be that two, or four trowels. Four would be very rare indeed.
I have absolutely no interest in polishing/shining work up, it's not supposed to be.
So basically the customer tells u how to do your job lolIf a customer says ohh I want it shiny and oh I love it when its all smooth and shiny
.I'm shining the s**t out of it,don't care if its not meant to be there have asked so il deliver shine.you can't tell some people there think your fobbing them off and if its not shiny and smooth there will complain.i couldn't give 2 hoots if paint dosnt adhere to the wall and needs a extra 2 coats of paint,not my problem and I've been paid leaving what there have asked for and thinking is right.its ill informed on there part thinking it needs to be like a mirror
Not what I said.if I la de da customer says can you make it nice n smooth and shiny,I say I can but it dsnt really need it as ull be putting a matt paint on there are not bothered and nor am I in the slightestSo basically the customer tells u how to do your job lol
If a customer mentioned shininess to me they'd get a full explanation if necessary, including being shown the relevant text from the NHBC, BS and BG.If a customer says ohh I want it shiny and oh I love it when its all smooth and shiny
.I'm shining the s**t out of it,don't care if its not meant to be there have asked so il deliver shine.you can't tell some people there think your fobbing them off and if its not shiny and smooth there will complain.i couldn't give 2 hoots if paint dosnt adhere to the wall and needs a extra 2 coats of paint,not my problem and I've been paid leaving what there have asked for and thinking is right.its ill informed on there part thinking it needs to be like a mirror
You’re such a geek AndrewIf a customer mentioned shininess to me they'd get a full explanation if necessary, including being shown the relevant text from the NHBC, BS and BG.
I really don't care that much about plasteringIf a customer mentioned shininess to me they'd get a full explanation if necessary, including being shown the relevant text from the NHBC, BS and BG.
Whether you care or not, I wouldn’t have misses Jones telling me how to finish a wall, u sound like a rite melt, mr kinkyI really don't care that much about plastering
I'm the biggest melt there isWhether you care or not, I wouldn’t have misses Jones telling me how to finish a wall, u sound like a rite melt, mr kinky
Went back before job only local didn’t have phone brilliant looking finish fella wants more rooms doing because of the finish .I’m happy I’ll take a photo on Monday when I’m back
Yeh they got yellow sticker on it saying 17 lites of water Needed lol,plus the batch date is late November - not OctoberHow do you know if its the first bad batch or second good batch?...are the bags any different?
So this gear has went from total shite,to very good in batch 2. ?Went back before job only local didn’t have phone brilliant looking finish fella wants more rooms doing because of the finish .
I shall not be trying it anytime soon..i rang a yard today as got a whisper there had 7 pallets in,anyhow said how much a bag and they said £12 per bag cash only..tried giving me the shite of there know a client who had 2 pallets left over and was instructed to sell it.bolloxsSo this gear has went from total shite,to very good in batch 2. ?
weres these pictures thenWent back before job only local didn’t have phone brilliant looking finish fella wants more rooms doing because of the finish .
Haha thats funnyCan see all Asians now calling family meeting..Abdul call Muhammed we have a meeting,bg are delivering bare plaster at end of August innit
Very surprised how good it looks once dry went over board today which I found a bit trickier but hopefully good when dry.Does dry out nice with the looks of it
End of day its trial and error its new stuff..i just can't be arsed trying a new productVery surprised how good it looks once dry went over board today which I found a bit trickier but hopefully good when dry.
They do a board plaster as well,never seen it or heard anyone saying they have tried it.Very surprised how good it looks once dry went over board today which I found a bit trickier but hopefully good when dry.
I've heard they do a unfinish one aswellThey do a board plaster as well,never seen it or heard anyone saying they have tried it.
Haven’t seen it yet ! Think I’ll try and master the multi first .They do a board plaster as well,never seen it or heard anyone saying they have tried it.
There's cynical old me thinking you was a rep for mg....sir I give you my sincere apologiesI have tried the board finish but probs wouldn’t use it again now as there new multi onto board is faster. Iam plastering a church hall with the New MG as the Customer couldn’t get 30 bags of BG. I was A bit unsure at first about doing the big high walls with it but its looking nice I’ll upload some pics tomorrow. The white finish is
Lol! Apology acceptedThere's cynical old me thinking you was a rep for mg....sir I give you my sincere apologies
Yup , mine turned out lovely. Going back there tomorrow will take some pics
I tried it today only half a bag lol,it turns quicker basically I troweled up with sawn off speedskim st and when it was changing colour I used speedy again the s**t responded better to plastic in my opinionVery surprised how good it looks once dry went over board today which I found a bit trickier but hopefully good when dry.