Well plastering since left school so 14 years now, In Cumbria we all seem to be stuck in the times myself included, Still apply 2 coats by hand and flatten with trowel then 2 wet rubs with trowel followed by a hard rub with trowel, Using a 14 or 16 inch steel marshalltown...
I know there is nothing wrong with this method and my work is very high standard but would love to make life easier:RpS_laugh:
So been looking at speedskims for flattening in, any good?
Also what about these Refina PlaziFlex s*p*r*lex Skimming Trowel i have been seeing?
Do they really make life easier and also leave a very high standard?