Just finished excavating a floor ready for limecrete. I'm going to have 150mm compacted foamed glass, underfloor heating pipes followed by 75mm of limecrete. On top of this will be 20mm limestone pavers.
I came across this today where someone laid the pavers directly in to the limecrete.
https://limewindow.blog/2012/11/12/limecrete-floor-with-flagstones/
Seems like a great idea to me, saves on waiting for drying until floor surface goes down and also saves a little bit of head height loss.
Can anyone tell me any reason not to do it like this and wait for the slab to fully dry before laying the pavers?
I came across this today where someone laid the pavers directly in to the limecrete.
https://limewindow.blog/2012/11/12/limecrete-floor-with-flagstones/
Seems like a great idea to me, saves on waiting for drying until floor surface goes down and also saves a little bit of head height loss.
Can anyone tell me any reason not to do it like this and wait for the slab to fully dry before laying the pavers?